PCB etching w. hardware store muriatic acid

Z

zxcvbob

Guest
....and 3% hydrogen peroxide from the drugstore? What ratio, and will it
work at room temperature?

If cheap 3% peroxide is not strong enough, what about ammonium nitrate
or potasium nitrate in dilute muriatic (hydrochloric) acid? That should
be functionally equivalent to dilute nitric acid.

I'm looking for something easy to get and less messy than ferric
chloride, and I don't even know where to find ammonium persulfate.

Thanks, and best regards,
Bob
 
I don't even know where to find ammonium persulfate.
Bob (zxcvbob)
Google is your friend.
http://groups.google.com/groups?&threadm=f8b945bc.0404071605.1fb8fb2e%40posting.google.com
 